J. Manuf. Sci. Eng. April 2007, 129(2): 311–318.
Published Online: September 20, 2006
.... The primary parameters varied in experiments were those found to most affect bonding between droplets: droplet temperature ( 250 - 345 ° C ) , substrate temperature ( 60 - 200 ° C ) , and deposition rate ( 1 - 15 Hz ) . At lower deposition rates the substrate cooled down too much to induce remelting whereas...